- Titanium Anode for Copper Foil
- 2020-09-25 09:35
- The pretreatment of electrolyzing copper foil---Titanium Anode1.Electrolyte :H2SO4(30%)+CuSO42.Current Density:3000A/M3.Working Temperature:60℃4.Service Life:≥2 Years(40 million hours)5.Ph Value:Highly Acidic6.Main Compositions:IrO2+X
- titanium electrode for swimming pool
- 2020-08-09 09:38
- Electrolytic preparation of titanium anode for sodium hypochloriteBase material: Gr1 titanium plate/meshCoating; Ruthenium-iridium
- Barrel Titanium Mesh Electrode/ anode
- 2020-06-24 19:58
- Substrate: Gr1 titanium> 99.6%Regular size of titanium mesh: 3 * 6/4 * 8 / 4.5 * 12.5Coating Type: Ru/Ir oxide coating, Ir/Ta coating, Platinum coating
- Ruthenium Series Mixed Metal Oxide Coated Titanium Anode
- 2020-06-23 05:31